This is the third one of these I’ve made, and I Think it turned out better than the previous one, which I have pictured on my website. All of them so far have been made as gifts for very special people. I tried to make the design such that it can be aesthetically pleasing whether it is being viewed as a religious symbol or having no symbolism at all. Made from three pieces of 16 gauge brass sheet formed into tubes and then twisted together. It is made to hang on a wall. Dimensions: about 9″ x 13″.










{ 1 trackback }
{ 1 comment… read it below or add one }
LynnWhite 12.03.08 at 11:34 am
I think these crosses are wonderful. I have been folowing your blog and really enjoy your pet urns. I took a look at your website today and saw lots of great art. You are an inspiration to me and, by the way, I enjoy nature as much as you do.